Rosswag qualifies another nickel-based superalloy for AM – Waspaloy

Metal processing company Rosswag Engineering has just qualified a new nickel-based superalloy – Waspaloy – for the laser powder bed fusion AM process. The German metallurgy specialist is one of the industry leaders in forging technology and material testing, having successfully processed and 3D printed the superalloy along with over 35 other alloys in recent […]